ASTM A202 Grade B is a chromium-manganese-silicon low-alloy steel tailored for high-pressure, medium-temperature pressure vessel applications.2026-04-30
-
ASTM A202 Grade A is a critical chromium-manganese-silicon low-alloy steel plate specifically designed for welded pressure vessels and boilers operating at medium temperatures.2026-04-30
-
ASTM A202 Pressure Vessel Steel Material and Grades:
Alloy System: **Chromium-Manganese-Silicon (Cr-Mn-Si)** Low-Alloy Heat-Resistant Steel2026-04-17 -
ASTM A204/A204M Grade B molybdenum alloy steel plates for pressure vessels feature superior chemical composition and mechanical properties compared to Grade A2026-04-10
-
As a molybdenum-alloy steel plate for pressure vessels under the ASTM A204/A204M standard, A204 Gr.A is a low-alloy, high-strength material specifically designed for service conditions involving moderate temperatures (≤400°C) and moderate-to-high pressure2026-03-31
DIN 17165 17 Mn 4, Grade 17 Mn 4, 17 Mn 4 steel
DIN 17165 17 Mn 4 steel is a kind of material for boiler and pressure vessel steel. So, DIN 17165 17 Mn 4 steel is used above all for manufacturing boilers, pressure vessels and pipes transporting hot liquids.
In addition, DIN 17165 17 Mn 4 steel is widely used in heat exchangers, weldable pressure vessels and boilers and pipework.
BEBON INTERNATIONAL is committed to steel processing and export. We have the most comprehensive service. One package service will be offered, including cutting,welding, drilling, shot blast cleaning, derusting, painting, galvanized, etc, our service will be around your requirement and ensure the perfect service. About DIN 17165 17 Mn 4 steel, we can offer the followspecification:
Thickness: 5-700mm
Width :1500-4020mm
Length:3000-18800mm
DIN 17165 17 Mn 4 steel chemical composition:
|
Grade |
C. % |
Mn.% |
S. |
N |
Cu |
Nb |
Ti. |
Si. |
P. |
AL |
Cr. |
Mo. |
Ni |
Vi |
|
17 MN 4 |
0.08-0.2 |
0.90-1.50 |
0.015 |
0.012 |
0.30 |
0.020 |
0.03 |
0.40 |
0.025 |
0.020 |
0.30 |
0.08 |
0.30 |
0.02 |
DIN 17165 17 Mn 4 steel mechanical property:
|
Grade |
Type |
Thickness mm |
Yield strength Mpa(min) |
Tensile Strength MPa |
Elongation % (min) |
Impact Energy (KVJ) (min) |
||
|
-20° |
0° |
+20 |
||||||
|
17Mn4 |
Normalized |
t≤16 |
295 |
460-580 |
21 |
27 |
34 |
40 |
|
16<t≤40 |
290 |
460-580 |
21 |
27 |
34 |
40 |
||
|
40<t≤60 |
285 |
460-580 |
21 |
27 |
34 |
40 |
||
|
60<t≤100 |
260 |
460-580 |
21 |
27 |
34 |
40 |
||
|
100<t≤150 |
235 |
440-570 |
21 |
27 |
34 |
40 |
||
|
150<t≤250 |
220 |
430-570 |
21 |
27 |
34 |
40 |
||
DIN 17165 17 Mn 4 equivalent material:
|
DIN 17165 17 Mn 4 equivalent material |
||||||
|
Europe |
Germany DIN |
Japan JIS G |
USA |
|||
|
EN10028-2 |
EU 113 |
17135 |
17102 |
3115 |
3103 |
ASTM |
|
P295 GH |
FeE315 KG,KW,KT |
A St 45 |
St E 315 |
SPV 315 |
SB450 |
A515gr.55,60,65,70 |
As a professional global 17 Mn 4 steel plate supplier, we promise we can offer you the qualified 17 Mn 4 steel plate and our 17 Mn 4 steel plate price is reasonable. If you have any confusion in 17 Mn 4 steel plate technical conditions, please contact us freely.